Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

The rubber liner butterfly valve torque will go up or down

Status
Not open for further replies.

bao2ye

Chemical
Joined
Mar 31, 2006
Messages
59
Location
US
Normally how long is the lifetime for an EPDM liner. Will the torque goes up with the aging of the EPDM liner for butterfly valve?

Thanks
 
EPDM liner will last for years on a water service.
It will be ruined after a few minutes if the service contains hydrocarbons. Or if (as I have seen) the maintenance apes lubricate them with diesel fuel when installing them in the valve body. Proper assembly lube: silicone grease. Even soapy water is good. Not diesel fuel or other petroleum product. Hydrocarbons make EPDM swell and get soft. A year or so on low-pressure steam less than 250F(120C)
If the service is gritty, reduce the OD of the vane to keep it from scrubbing the grit into the vane. (Called Undercut disc) This reduces the pressure limit at which the valve will shut off, but at low pressures (less than about 75 psi) it lasts longer and requires less torque with unndercut disc.


 
Does anybody know a website showing a picture or a sketch of an "undercut disc"?

Many thanks in advance, 'NGL
 
They look just like any other disc. They just have a slightly smaller OD.
 