Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

The cheapest methods to make this FPV Drone frame parts that are made from super stiff carbon?

Status
Not open for further replies.

Imposter666

Mechanical
Joined
Jan 15, 2021
Messages
36
Location
CA
I would like to design and possible mass produce an FPV drone that will have a similar parts made out of super stiff carbon like the one you see in the link: What is is the best and cheapest manufacturing technique to make these? Waterjet, laser cut, CNC? Maybe I am missing a method that I should consider?
 
Chimera7-Pro-Side-Plate_ytb6eo.jpg

Nothing to add other than these pieces are almost certainly molded, possibly CFRP.
 
Carbon fibre parts are not "cut" or "machined" to shape. They are built up - either as true "molds" or as additive manufacture. This is because the grain orientation of the fibre is what gives it the strength: if machined after the fact, the probability is non-trivial that a large number of these strands will be broken or otherwise damaged, thereby reducing the allowable stress concentrations drastically. l

Converting energy to motion for more than half a century
 
That looks like an injection molded part that is not intended to be super- strong or stiff. Chopped glass or carbon fiber in the molding resin will make it significantly stronger and stiffer, but not like one made from continuous fiber, which this is not.
 