Hello,
I am quite new here so sorry If this question was answered already, but I can not find it.
API 1104 is new for me as well so please advise me as follows:
If you qualify PQR for pipe with all test: VT, RT plus others DT. Can you use automatic UT during production or you have to use the same volumetric test as for qualification?
I used to work with EN and for me it should be no problem (both are volumetric) but it is always better to ask.
Thanks...
I am quite new here so sorry If this question was answered already, but I can not find it.
API 1104 is new for me as well so please advise me as follows:
If you qualify PQR for pipe with all test: VT, RT plus others DT. Can you use automatic UT during production or you have to use the same volumetric test as for qualification?
I used to work with EN and for me it should be no problem (both are volumetric) but it is always better to ask.