For rewind of a 25kv 1000+MW generator using local vpi epoxy resin insulation system, I am interested in learning what strategy is used for testing sample coils:
1 - Assuming we request supplier to provide 2 or 4 extra bars, how do you select bars to test? Random? Lowest power factor?
2 - What type of test would you recommend to be performed on the sample coils.
3 - A manager asked me if I agree with the following tests recommended by a vendor: voltage endurance, TVA probe, partial discharge, and "CNDF"....what the heck is CNDF? I assume maybe it has something to do with Dissipation Factor (power factor).
4 - I know for motors we typically do dc hi-pot to failure and if that doesn't fail it then surge test to failure. Then we dissect the coil at strategic locations including near the location of the failure where we are more likely to find voids / weaknesses. I know surge test is not applicable to bars which have one (half) turn. What type of destructive electrical test would you recommend to find weak spots to dissect on a Roebel bar ?
=====================================
(2B)+(2B)' ?
1 - Assuming we request supplier to provide 2 or 4 extra bars, how do you select bars to test? Random? Lowest power factor?
2 - What type of test would you recommend to be performed on the sample coils.
3 - A manager asked me if I agree with the following tests recommended by a vendor: voltage endurance, TVA probe, partial discharge, and "CNDF"....what the heck is CNDF? I assume maybe it has something to do with Dissipation Factor (power factor).
4 - I know for motors we typically do dc hi-pot to failure and if that doesn't fail it then surge test to failure. Then we dissect the coil at strategic locations including near the location of the failure where we are more likely to find voids / weaknesses. I know surge test is not applicable to bars which have one (half) turn. What type of destructive electrical test would you recommend to find weak spots to dissect on a Roebel bar ?
=====================================
(2B)+(2B)' ?