We have a large fleet of Nitrogen hoses that has a brass end connector fitted onto it. This brass end connector are silver soldered to the hose end pipe. Brass end are smallest part.
Currently we are doing this without any other means of Q.C than pressure testing and using high skilled welders.
Is there any ways we can test this?
The connector is 1-1/4" OD, pressure is up to 300 psi, medium is liquid Nitrogen (-196 degree C). so the consequences of a failure is rather worrying.
Alternative is ofcourse to start threading the connections and/or changing them with stainless steel, but the cost impact is significant
Currently we are doing this without any other means of Q.C than pressure testing and using high skilled welders.
Is there any ways we can test this?
The connector is 1-1/4" OD, pressure is up to 300 psi, medium is liquid Nitrogen (-196 degree C). so the consequences of a failure is rather worrying.
Alternative is ofcourse to start threading the connections and/or changing them with stainless steel, but the cost impact is significant