Hi all,

I have carried out several torsion tests on toughened and laminated glass beams. The shear modulus values calculated from these seem fine, but I am looking to verify these against other shear test methods for toughened glass now. So far haven't found too much as far as standard test procedures go .. is anyone familiar with any such details (shear block test etc)? Thanks.

Regards,
KU.
 
Old Reference... may/may-not be useful...

MIL-HDBK-722 GLASS
Chapter 6 Quality Assurance....
Functional Tests

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top