I have a product that consists of two handle halves screwed together with a rubber gasket compressed in a channel between them. There are also 3 rotary spring seals over shafts on one handle half.

I am looking for suggestions on the best way, in a manufacturing clean room environment, to do an in process test to evaluate whether our seals are installed properly. The condition these are designed for is a 35 psi gage steam pressure for several minutes followed by a vacuum.(For those familiar with the medical world this is an autoclave cycle)

I'm looking at alternatives to simulate this cycle in process.

Should I pressurize the inside and look for pressure decay? (inside pressure reduces bolt compression)

Should I put in a chamber with vacuum(can't reach 35 psi differential with vacuum)

Should I submerge in liquid? (possible damage to electronics internally)

Thanks for any help you can provide.
 
Replies continue below

Recommended for you

There are lots of commercial leak detectors. Pressure is always easier than vacuum. I prefer flow meters to pressure decay but they cost more.

Liquid submersion is always my last choice.
 