We have a new product line of butterfly valves. I have designed and built fixtures for testing all sizes 2" - 10" that will run on our existing test stands. None of our test stands had the required ram force to hydro-test our 12"-16" sizes at 400 psi. Since these are low volume we decided not to invest in a new test stand. Instead, I had one of our sister companies design special blind flanges to bolt to either side of these valves for testing. When I ran a test on the 12" I blew out my 90A Urethane seal immediately. I know that 400psi in a 12" valve exerts a force in excess of 45000 lbs. How can I calculate the force that these bolts are putting on the valve when torques to 125 ft lbs? Also, Are there ant calculations for the elongation of Nitronic 60 studs under load? These would help me to make sure I am putting enough pressure on the seals. Any other tips you can provide on testing butterfly valves of this size would be appreciated.
Thanks
Thanks