Aug 7, 2001 #1 satchit Electrical Joined Aug 7, 2001 Messages 2 Location IN Can anyone guide me in deciding the rate of loading for tensile test of Mild steel specimen? Is there any reference which gives details of such information?
Can anyone guide me in deciding the rate of loading for tensile test of Mild steel specimen? Is there any reference which gives details of such information?
Aug 7, 2001 1 #2 Ron Structural Joined Sep 24, 1999 Messages 16,336 Location US Use ASTM Test Method E8-00b, Standard Test Methods for Tension Testing of Metallic Materials Upvote 0 Downvote