Can anyone guide me in deciding the rate of loading for tensile test of Mild steel specimen? Is there any reference which gives details of such information?
 
Replies continue below

Recommended for you

Use ASTM Test Method E8-00b, Standard Test Methods for Tension Testing of Metallic Materials
 