I am trying to calculate the tensile strength of a screw by taking the wire tensile strength and drawing it down thru a wire drawer and then cold heaing it. Example .224 302 wire 72ksi drawn down to .214 diameter and headed to .2150 dia. Is there a formula to determine how much tensile will increase per .001 that the wire is drawn?