I'm currently working on a stone panel job. Some of the stone is attached to the support structure with copper wire. I need to know the allowable tensile strength of typical copper wire. I'm having trouble finding the data.
 
buy some and pull it ...

googling "strength of copper wire" got some relevent hits ...
from wiki Q&A, with sensible cavets, 32ksi (i'd use 16ksi as a design guide)
 
That's how it's commonly attached and they've probably been doing it that way since Julius Ceasar's day, if not before. That's not to say don't run the numbers, but do take some comfort in knowing that if an experienced stone mason is involved he may well have hung many such panels that way over his career.
 
I know it's going to work but I am not the PE signing this and I have to prove through calcs that it works. I'm going to use the minimum value in a Mech. of Materials text book. It's an interior panel and only seeing 5 psi wind pressure.

Thanks
 
But, any dentils are probably on the outer surface of the stone panels, not on the back surface. So the floss probably won’t work.
 