Hi All :
There are two aluminum pipe pieces having a 1" gap between them and this gap is covered by Ventglas Wrapped around it. Helium gas with a pressure of 35 psi flows through the pipe. My task is to find out what the maximum gap can be without the Ventglas failure.
Now, the strength of ventglas is given as 480lbs/inch in the warp and 360lbs/inch in the filling. What does this means ? What does it mean to have tensile strength in lbs/in rather than psi ?
Thanks,
Kapil,EWI