For procedure qualification per ASME Section 9 and regarding the tensile acceptance criteria, why the code accepts 5% below the the minimum specified tensile strength of the base metal if the sample brakes out of the weld. Contrarely it tolerates not less than the minimum specified tensile strength if it breaks in the weld ?