We are fitting & welding a large vessel. Plate thk.
is 1.625 in.The weld joints are being fitted & temporary
steel fit up attachments with a 'rat hole' or weld access hemi hole in the attachment are being welded to the two plates on each side of the weld joint to maintain the alignment. The plates are then being tack welded & then the root, 2nd, & 3rd pass is deposited. Then the joint is being back gouged & welded on the opposite side.Then the opposite side is welded to completion. My question is when should the welded clamps be removed?
is 1.625 in.The weld joints are being fitted & temporary
steel fit up attachments with a 'rat hole' or weld access hemi hole in the attachment are being welded to the two plates on each side of the weld joint to maintain the alignment. The plates are then being tack welded & then the root, 2nd, & 3rd pass is deposited. Then the joint is being back gouged & welded on the opposite side.Then the opposite side is welded to completion. My question is when should the welded clamps be removed?