im trying to design a glass roof and i need to calculate the udl due to each pane of glass and i am trying to establish values for the density, thickness , tenscile strenth and available areas for products currently available on the market, any help much appreciated
 
Common glass weighs 156 pounds per cubic foot, if that's any help.
 