Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

temperature vs.yield strength reduction 2

Status
Not open for further replies.

chrislaope

Structural
Joined
Sep 15, 2010
Messages
89
Location
US
I am designing a structural steel frame (AISC C Channel Fy=36ksi) which will work under 400---500 F degree. I am trying to find how much yield strength will be reduced under this temperature. Can anybody shed some light on it?

many thanks.
 
The AISC 13th edition steel manual has a section on Thermal Effects (page 2-31 through 33). They reference Design Guide 19 (which I do not have) for applications involving loading at elevated temperatures.
 
Chris:
As JoshP mentions, the AISC Manual has always had some discussion on temperature and how it effects structural steel. Modulus of Elasticity starts decreasing slowly with temp. elevations above room temp. And yield and tensile strengths start decreasing at about 600-700°F. The attached is from “Structural Steel Designers’ Handbook,” Edited by Frederick S. Merritt, Pub. by McGraw-Hill.
 
 http://files.engineering.com/getfile.aspx?folder=7301911b-e704-4739-bd20-9c89f9af50e7&file=Temps..pdf

Thanks guys, your information is very helpful.
 