Dec 27, 2017 #1 Moossii Chemical Joined Dec 27, 2017 Messages 4 Location QA Hello, Where should I look to find out the minimum temperature rating of SA 516 Gr 60?
Dec 27, 2017 #2 JStephen Mechanical Joined Aug 25, 2004 Messages 8,743 Location US Is this an ASME vessel or what? Upvote 0 Downvote
Dec 27, 2017 Thread starter #3 Moossii Chemical Joined Dec 27, 2017 Messages 4 Location QA Yes sir. The ASTM equivalent is A 516 Gr 60 Upvote 0 Downvote
Dec 27, 2017 1 #4 r6155 Mechanical Joined Jan 12, 2010 Messages 3,031 Location AR Look at SA-20 Regards r6155 Upvote 0 Downvote
Dec 27, 2017 1 #5 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US If you mean the lowest permitted temperature that will depend on material thickness and heat treatment in ASME Section VIII, Div 1. Upvote 0 Downvote
If you mean the lowest permitted temperature that will depend on material thickness and heat treatment in ASME Section VIII, Div 1.
Dec 27, 2017 1 #6 weldstan Materials Joined Jun 24, 2011 Messages 2,809 Location US See UCS-66. Look at the curves in the figure therein. Upvote 0 Downvote
Dec 31, 2017 Thread starter #7 Moossii Chemical Joined Dec 27, 2017 Messages 4 Location QA Thankyou All Upvote 0 Downvote