Jul 1, 2015 #1 paddy1385 Mechanical Joined May 4, 2015 Messages 12 Location GB Hi, Can anyone please advise me temperature range for B7/2H HDG fasteners, I have ambient temp. of -25 Deg C, so was worried if it can work at this low temperature. Also if I use A320 L7, will there be huge cost impact.
Hi, Can anyone please advise me temperature range for B7/2H HDG fasteners, I have ambient temp. of -25 Deg C, so was worried if it can work at this low temperature. Also if I use A320 L7, will there be huge cost impact.
Jul 1, 2015 #2 desertfox Mechanical Joined Dec 29, 2002 Messages 5,559 Location GB http://www.mts.com.sa/en/product/stud-bolts/b7-studbolts-b7-threaded-tods-2h-hexagon-nuts “Do not worry about your problems with mathematics, I assure you mine are far greater.” Albert Einstein Upvote 0 Downvote
http://www.mts.com.sa/en/product/stud-bolts/b7-studbolts-b7-threaded-tods-2h-hexagon-nuts “Do not worry about your problems with mathematics, I assure you mine are far greater.” Albert Einstein