Pls find below Temperature limitation followed by an XYZ organization in designing the Boiler Pressure parts.
SA 106 Gr.B <425 Deg Cel
SA 335 Gr.P11 <510 Deg Cel
SA 335 Gr.P22 <560 Deg Cel
SA 335 Gr.P91 <560 Deg Cel
Can anyone please explain what is the basis of limiting the temperature based on Materials (ASME Code) ?
Thanks in advance
kind Regards,
R.Ilanseran
Pls find below Temperature limitation followed by an XYZ organization in designing the Boiler Pressure parts.
SA 106 Gr.B <425 Deg Cel
SA 335 Gr.P11 <510 Deg Cel
SA 335 Gr.P22 <560 Deg Cel
SA 335 Gr.P91 <560 Deg Cel
Can anyone please explain what is the basis of limiting the temperature based on Materials (ASME Code) ?
Thanks in advance
kind Regards,
R.Ilanseran