Feb 7, 2024 #1 Waqas-999 Mechanical Joined May 18, 2023 Messages 5 Location PK My question is there any upper temperature limit up to which ASME section viii division 1 can be applied. or there is no such limit
My question is there any upper temperature limit up to which ASME section viii division 1 can be applied. or there is no such limit
Feb 7, 2024 1 #2 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,841 Location US Waqas-999, no upper temp limit as such in Sec VIII, Div 1, but rather upper temperature limits for materials as shown in Sec II, Part D. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand Upvote 0 Downvote
Waqas-999, no upper temp limit as such in Sec VIII, Div 1, but rather upper temperature limits for materials as shown in Sec II, Part D. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand
Feb 7, 2024 #3 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,115 Location NL The highest you can (currently) go is 982 deg C or 1800 deg F. Huub - You never get what you expect, you only get what you inspect. Upvote 0 Downvote
The highest you can (currently) go is 982 deg C or 1800 deg F. Huub - You never get what you expect, you only get what you inspect.
Feb 24, 2024 Thread starter #4 Waqas-999 Mechanical Joined May 18, 2023 Messages 5 Location PK @XL83NL which clause of the code says that. or if it is from some other literature kindly mention it as well. Thank you Upvote 0 Downvote
@XL83NL which clause of the code says that. or if it is from some other literature kindly mention it as well. Thank you
Feb 24, 2024 #5 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,115 Location NL It’s from ASME IID, where the tables list the max temperature for the material under consideration, per the applicable design Code (column wise). Look e.g. for UNS N06617. Huub - You never get what you expect, you only get what you inspect. Upvote 0 Downvote
It’s from ASME IID, where the tables list the max temperature for the material under consideration, per the applicable design Code (column wise). Look e.g. for UNS N06617. Huub - You never get what you expect, you only get what you inspect.