We tried teflon coated bolts on some of our more corrosive services year and years ago and saw no real increase in corrosion resistnace or bolt life. I understand that advances may have been made in the area since we tried them. How much benifit are people seeing in bolt life in HCL, caustic and other coorosive services with teflon coated bolting in real life plant environments
Thanks
Thanks