Trying to remove Tedlar film Coating From A CFM56 Fan Outlet Guide Vane (Dupont TTY 40 BE 5). We have tryed to remove using plastic blast media, but find it extremely time consuming, and there is a chance of damaging the Kevlar substrate. Have also tryed soaking the part in MEK, but this also did not help to soften the film.

Anybody?
Best Regards



 
Replies continue below

Recommended for you

Have you checked with Cytec Engineered Materials in Havre de Grace, Maryland? They are the Tedlar manufacturers.
 