Hi,
Does anyone know if Techlok and Graylok Hubs are the same piece piece of equipment albeit from a different manufacturer? are they interchangeable if they are the same size, can one style be used to replace the other?

Thanks
 
Replies continue below

Recommended for you

Only as a pair.

The previous post still applies AFAIK.

In reality the two may work but as they are not made to an official standard then there may be subtle differences which cause it not to work properly.

Unless you can get this in writing from the vendors then you're out on a limb. I couldn't find anything which says you can use them interchangeably.

Let us know what you find. [pre][/pre]

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 