If the e/D is 2 or greater, do you have to worry about tearout failure or not? One of my team mates says that, if e/D is 2 or greater then, fatigue is not an issue, but tear out failure should be calculated. Can anyone help. Thanks
 
In what sheet material? what thickness? single shear or double shear?

Don't think you can make a blanket statement about fatigue; depends on joint config, material, fastener, loading spectrum, etc, etc.

Why not just calculate the tear out as well as bearing static margins?
 
Gotta' agree with SWComposites. To make a blanket statement like this doesn't make sense. Each situation is different. If you are using 0.032" sheet to try and repair a skin on a commercial aircraft...probably not going to work. Using it on an ultralight? Different story.

2D is a good "rule of thumb", but you still need to do your "due diligence".

Garland E. Borowski, PE
Engineering Manager
Star Aviation
 
and what's the connection between shear-out and fatigue ?

i would always check shear-out as one of the possible modes of failure.

fatigue is an altogether different thing, sure with a reasonable edge distance the Kt is pretty much 3 (for an open hole) but not something i'd dismiss. possibly not something i'd spend a ton of time on either ... it depends on the structure involved.
 
Hart-Smith recommended a 3d edge distance to prevent shear-out and a pitch of 5d to force bearing failure in preference to tension-through-hole failure.
 