We are specifying the new TCP conversion coating for some alumium parts and we have always specified "gold" color to our CR(6) coatings. I understand adding dyes to TCP makes it fail salt spray tests. We don't need a lot of protection since the end product is used in laboratory conditions. Will platers be adding color to TCP coatings if it is specified?