Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

TC40/41 Flaking

Status
Not open for further replies.

Vig16

Mechanical
Mar 21, 2007
67
We had some of our 17-4 PH Stainless Steel recently coated with TC40 and TC 41 films. The coating was fine when we received it, but it started to flake as we started passing another metal along it (it's used as a clamping jaw in a feeder system with metal clips). The 17-4 was solution annealed before being coated.

The question is, what could have gone wrong in the process? Also, what can be done to fix it?

The 17-4 is coated to lower friction as well as increase the surface hardness.

Thanks!
 