Have a condition that requires the replacement of 400 A490 1" TC bolts. Upon removal the nuts and washers will not be in as-manufactured condition (clean/lubricated) so they can not be reused, correct?
Specification for Structural Joints Using ASTM A325 or A490 Bolts
2.3.3. Reuse: ASTM A490 bolts and galvanized ASTM A325 bolts shall not be reused.