We need to connect the skirtings for 30" bus ducts to the wall of the isophase box. Details as follows:
Wall is 1/2" thick in 6061 aluminum. Bolt groups are 24 - 3/8" dia on 18" radius. Design loading achieved 20 times in life. At other times, nominal loading only but box continually vibrating. Open to weather in medium industrial setting (30 yrs design life).
Can you advise:
Is it safe to tap the aluminum wall, or must we use through bolts?
What material for the bolt (inc nut, washers, gaskets if used).
Wall is 1/2" thick in 6061 aluminum. Bolt groups are 24 - 3/8" dia on 18" radius. Design loading achieved 20 times in life. At other times, nominal loading only but box continually vibrating. Open to weather in medium industrial setting (30 yrs design life).
Can you advise:
Is it safe to tap the aluminum wall, or must we use through bolts?
What material for the bolt (inc nut, washers, gaskets if used).