Jul 7, 2021 #1 ilkin014 Materials Joined Jan 7, 2017 Messages 2 Location AO HI All, Could you please advise me, which types of metallurgical affects has a taper boring on fittings/flanges (for Carbon and Stainless Steels)? (For example if we are going to reduce wall thickness up to 10mm?) Regards, Ilkin HASANOV.
HI All, Could you please advise me, which types of metallurgical affects has a taper boring on fittings/flanges (for Carbon and Stainless Steels)? (For example if we are going to reduce wall thickness up to 10mm?) Regards, Ilkin HASANOV.
Jul 7, 2021 #2 LittleInch Petroleum Joined Mar 27, 2013 Messages 22,990 Location GB I don't understand the question. Taper boring is a machining issue where if you lubricate the cutting element, there is no impact. 10mm sounds like a lot though. Most flanges have min and max bores which may not accomdate that much. Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
I don't understand the question. Taper boring is a machining issue where if you lubricate the cutting element, there is no impact. 10mm sounds like a lot though. Most flanges have min and max bores which may not accomdate that much. Remember - More details = better answers Also: If you get a response it's polite to respond to it.
Jul 9, 2021 #3 GD2 Mechanical Joined Sep 25, 2017 Messages 725 Location CA Ilkin014, Look up the flange/fitting standards and see what is the minimum required thickness. Simply put, going below the required thickness is not acceptable unless you want to spend expensive engineering analysis. GDD Canada Upvote 0 Downvote
Ilkin014, Look up the flange/fitting standards and see what is the minimum required thickness. Simply put, going below the required thickness is not acceptable unless you want to spend expensive engineering analysis. GDD Canada