Hello All,
I am a Green Horn, Mechanical Engg.(10 month old in Proff.career). I am preparing Eng-Specification for the shell and Tube Heat exchanger.
This one is small size exchanger(AEL Type-Shell & tube 1 Pass each) ( over all Surface area 143 sq.ft) w/Tube Length 10 ft , No of Tubes =109) Design temp= 250 dg F and Design press= 150 psig /FV(shell side) & 150 psig (Tube side).
Material's are as follows:
Tubes: Tantalum
Shell: Carbon steel
Tubesheet: Haste alloy C276 (Claded with Tantalum)
Flanges & Channels: Haste Alloys w/ Tantalum Liner
Here are the Array of questions:
1) What should I include in my Eng-Spec as far as testing for the Tantalum tubes are concern. What are the important point’s should i need to include in my specification, concerned to the Tantalum Tubes Testing, Welding. Is there any special procedure that I need to include in my specification?
2) I am looking at two options for Tube sheet?
* Clade the Haste alloy C276 Tube sheet w/ Tantulum
* Is it okay to weld overlay to the Tube Sheet instead?
* Lines the Tube sheet w/ Tantalum (Is this same as cladding??)
Which option is much better and cheaper?
Please Guide.
Thanks a lot in advance.
Mechmania
I am a Green Horn, Mechanical Engg.(10 month old in Proff.career). I am preparing Eng-Specification for the shell and Tube Heat exchanger.
This one is small size exchanger(AEL Type-Shell & tube 1 Pass each) ( over all Surface area 143 sq.ft) w/Tube Length 10 ft , No of Tubes =109) Design temp= 250 dg F and Design press= 150 psig /FV(shell side) & 150 psig (Tube side).
Material's are as follows:
Tubes: Tantalum
Shell: Carbon steel
Tubesheet: Haste alloy C276 (Claded with Tantalum)
Flanges & Channels: Haste Alloys w/ Tantalum Liner
Here are the Array of questions:
1) What should I include in my Eng-Spec as far as testing for the Tantalum tubes are concern. What are the important point’s should i need to include in my specification, concerned to the Tantalum Tubes Testing, Welding. Is there any special procedure that I need to include in my specification?
2) I am looking at two options for Tube sheet?
* Clade the Haste alloy C276 Tube sheet w/ Tantulum
* Is it okay to weld overlay to the Tube Sheet instead?
* Lines the Tube sheet w/ Tantalum (Is this same as cladding??)
Which option is much better and cheaper?
Please Guide.
Thanks a lot in advance.
Mechmania