Hi,

API 653 Section a paragraph 4.3.3.1 a)when determining the minimum acceptable thickness for an entire shell course,t min is calculated as follows:

t min = 2.6(H-1)DG/SE

S=maximum allowable stress, E=joint efficiency, G=specific gravity of contents, H=height of the course in consideration

API 653 Table 4.1 gives the allowable stress for each course,allowable product stress and allowable hydro-static test stress(to be used if tank is subject for hydro test)

My tank is a water storage. Referring to the given formula,which allowable stress should be used in the formula?.Since the product is water,I used the maximum allowable for hydro-test and not the allowable product stress.Please comment if ever you found my judgement wrong or if Im missing something.I truly appreciate any reply.

best regards,
blawn

 
Use product stress for long term service. Use hydrotstatic stress for short term testing using water. In your case you should use product stress with SG=1.0 ( or slightly higher if sea water ). You could also use ADDA D-100 as your design code.
 
Sorry - AWWA, not ADDA in previous post.

You are using a out-of-date version of the code. The shell thickness equation is in 5.6.3.2. Don't forget to add corrosion allowance.
 