I have to repair an API tank 650 appendix F.
we want to do some lapped plates in the internal shell.
I am reading API 653 and I couldn not find if the lapped patch can we welded in the internal shell.
We want to do it in that way, just to avoid crevice corrosion for in case the patch is welded externally.
We read in the 9.3.1.6 a limitation in the internal shell patch of 6" distance from the shell to bottom weld.
Is correct to weld internally following the figure 9-1.?
Regards
Luis
we want to do some lapped plates in the internal shell.
I am reading API 653 and I couldn not find if the lapped patch can we welded in the internal shell.
We want to do it in that way, just to avoid crevice corrosion for in case the patch is welded externally.
We read in the 9.3.1.6 a limitation in the internal shell patch of 6" distance from the shell to bottom weld.
Is correct to weld internally following the figure 9-1.?
Regards
Luis