Tank Dent Aceptance Criteria

Status
Not open for further replies.

TANKO

Mechanical
Jan 20, 2011
32
Good Evening sirs,
what are the acceptance criteria for a tank vent?
During the construction, perhaps for a incorrect procedure welding of a stair support, we have suffered this distorsion.

thanks

regards

 
Replies continue below

Recommended for you

Atmospheric or pressurized tank? Shape of tank? Size of tank versus size of distortion?

Maybe check Roark's to see if there are any calculations for plate stress with distortions. If there isn't, you may be able to figure out residual stress from the dent and then use that to figure out total plate stress while the tank is at normal/max operating conditions.
 
Is it an API-650 tank? If so, have you checked the API-650 shell tolerances in that area?
 
TANKO,
What is distorsion or do you mean distortion?
 
API650, atmospheric and cylindrical shape 390m3..it's a small tank. The dent is about 300x300,on the 2°shell course
 
Also depends if this is a new tank ( use API 650 ) or an existing tank ( use API 653 )
 