Does anyone have any experience with external (UT) inspection of API650 tanks for corrosion of the annular plate?
I have an ø18m tank, 27 years old, carbon steel containing hot caustic soda solution. This cannot be taken out of service without vast expense. I am concerned over annular corrosion due to experience with other tanks on this site. I need to get some quantitative data on the condition of the tank. At present I have no data, so I cannot quantify the risk.
I have seen information about Lorus. Does anyone know if this acutally works?
Thanks in advance
I have an ø18m tank, 27 years old, carbon steel containing hot caustic soda solution. This cannot be taken out of service without vast expense. I am concerned over annular corrosion due to experience with other tanks on this site. I need to get some quantitative data on the condition of the tank. At present I have no data, so I cannot quantify the risk.
I have seen information about Lorus. Does anyone know if this acutally works?
Thanks in advance