I want to carry out UT in lieu of RT. Table UW-12 indicates joint efficiency values only if joint is radiographed. Where I could get joint efficiency values for UT joints?
 
UT is one of the NDE for inspection, but isn't credited for the joint efficiency.
 
Interpretation VIII-1-16-89 reads as follows:

Question: Do the joint efficiencies listed in Table UW-12 apply when ultrasonic testing is performed in lieu of radiographic examination, when allowed by UW-51?

Reply: Yes.

Hope this helps.
 
Is interpretation VIII-1-16-89 still valid under the current Code requirements, i.e. 2017 edition?
 

Jano6924 (Mechanical)- I donot find this interpretation in 2017 edition.

Please help.
 
Interpretations are not issued per edition. The important thing is that volumertic examination either RT or UT is performed. The Section VIII committee has not updated Table UW-12
 
How would VIII-1-16-89 be allowed under UW-11(a)? I see no general provision in there for UT, other than specifically addressed under UW-11(d)/(e)/(f)/(g).
 
XL83NL said:
How would VIII-1-16-89 be allowed under UW-11(a)? I see no general provision in there for UT, other than specifically addressed under UW-11(d)/(e)/(f)/(g).

Read UW-51(a)(4)
 
You can find this interpretation in the ASME web site using the following link:


I cannot talk about the 2017 edition of the code I still don’t get it. I understand that an interpretation remains valid until specifically annulled by the code, or implicitly annulled by other interpretation or by a revision or change in a VIII-1 paragraph.

Please take note that per VIII-1-16-89 interpretation the joint efficiencies of Table UW-12 can be used for ultrasonic testing ONLY WHEN ALLOWED BY UW-51.