When changing plastics in blow molding, polycarbonate to PETG, is it necessary to re-tool the mold? Any help on this would be appreciated. I have tried searching the forums, and do not know if I am using the correct search terms.

Thanks
 
Replies continue below

Recommended for you

PETG has a lot bless mould shrinkage than PET and is not all that different to PC. I would need to check data sheets for exact numbers. Eastman and Bayer should be able to provide reliable data to the exact difference in shrinkage.