Mere months following installation 6inch 900# CS BW sch120 leaked at its side flange. Valve is in boiler feedwater service exiting heater @1500psig,600degF fluid conditions. Need to how failure can happen assuming valve was not damaged going in? Any suggestions on this reknowned manufacturing job.
 
jerry, Check with your valve supplier. There's a lot of rebuilt crap coming in from overseas these days being sold as OEM. You may have gotten hold of one.

Hope this helps.
saxon
 
Jerry ...Just to make sure I got the story right, this is a 6"-900# welded end valve? ...SO, did any body check the bonnet bolts torque, before they commission this system? ...Or did they assume it was ok out of the box? ...Mark
 
What sort of failure was it? Did a stud or bolt fail? Did the bonnet crack? Did a gasket blow out? Something else?