Good morning,
As it is known, most spiral wound gaskets problems occur during installation? Is is possible to use even adhesive drops to help install them?
Additionally, we have a heat exchanger cap where the gap between its flange and tube sheet flange and we did all the recommended installing steps for the gasket and we still have some leaks.
We though of installing a weld ring gasket. So, any information on this type and how to dismantle the cap in the future when we use such type of gaskets?
Thanks a lot
As it is known, most spiral wound gaskets problems occur during installation? Is is possible to use even adhesive drops to help install them?
Additionally, we have a heat exchanger cap where the gap between its flange and tube sheet flange and we did all the recommended installing steps for the gasket and we still have some leaks.
We though of installing a weld ring gasket. So, any information on this type and how to dismantle the cap in the future when we use such type of gaskets?
Thanks a lot