We found evidence of hydrotreater feed mixing with the reactor effluent. The analisys showed that we have a leak in our feed/effluent exchanger train.
Is there a way to take reactor effluent samples during normal plant operation, between heat exchangers? There are 6 exchangers in total. We don't know which one is leaking and don't know how to identify the one that's leaking. Our plan is to hydrotest all of them.
If you of a way to take samples of reactor effluent between exchangers, please advise.

Krešimir Jedna?ak
 
If you don't have any bleeders, how on earth would you want to sample, let alone safely? Just take that unit down, hydrotest all the exchangers (who knows, there may be more than one leaking) and repair what needs to be repaired. If you try to be too intelligent, Murphy's law predicts you will have to shut down twice... ;-)
 
There are on line radioactive leak testing systems detection on heat exchangers that can have application in your unit

Tru Tec is a know technology please visit the site bellow maybe they can be of help



Regards

Luis Marques
 