Dear All
I would like to know your inputs about the following:
Some workshop received a two speed, two preformed windings 690-690 V generator. During the initial tests both windings were surge tested at 1500 V diagnostic was low speed winding burned.
Due to economic matters the costumer prefer to rewound only the low speed winding,then the work shop removes the low voltage winding and clean all surfaces deep. Again the good winding was surtested at 1500 V no problems were detected. High speed windig is at least 7 years old but was not overheated and with out any discolaration o posible failures in the winding.
The low voltage winding was installed and before varnishing both windings were surge tested at 5000 V with failure in the old high speed winding (Turn to Turn short circuit).
Seems is clear but please tell me your inputs about it.Also your experience surge testing old windings and voltage levels used for it.
Thanks in advance
Carlos
I would like to know your inputs about the following:
Some workshop received a two speed, two preformed windings 690-690 V generator. During the initial tests both windings were surge tested at 1500 V diagnostic was low speed winding burned.
Due to economic matters the costumer prefer to rewound only the low speed winding,then the work shop removes the low voltage winding and clean all surfaces deep. Again the good winding was surtested at 1500 V no problems were detected. High speed windig is at least 7 years old but was not overheated and with out any discolaration o posible failures in the winding.
The low voltage winding was installed and before varnishing both windings were surge tested at 5000 V with failure in the old high speed winding (Turn to Turn short circuit).
Seems is clear but please tell me your inputs about it.Also your experience surge testing old windings and voltage levels used for it.
Thanks in advance
Carlos