I looking for definition for black optical coating for aluminum parts,
for non-reflective surfaces, except black anodize.


 
Replies continue below

Recommended for you

What do you mean by "definition?" And why not black anodize?

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529

Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
 
There is one that I know is not a type of anodize:
Aeroglaze Z306 paint


Han primo incensus
 
Krylon ultraflat black used to be the standard paint for things like blackbodies, but some of its characteristics are dependent on proper application technique

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529

Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor