Sep 25, 2008 #1 chipgt500 Mechanical Joined Sep 25, 2008 Messages 3 Location US I have a drawing (in Japanese) that calls for a surface finish of "SBCr". The material is Nobinite CD-5 (similar to Invar 36). Does anyone know what process "SBCr" is referring to?
I have a drawing (in Japanese) that calls for a surface finish of "SBCr". The material is Nobinite CD-5 (similar to Invar 36). Does anyone know what process "SBCr" is referring to?
Sep 25, 2008 #2 ctopher Mechanical Joined Jan 9, 2003 Messages 17,519 Location USA, CA The only thing I can find on a quick Google search is some type of powder coating. Chris SolidWorks/PDMWorks 08 3.1 AutoCAD 08 ctopher's home (updated Aug 5, 2008) ctopher's blog SolidWorks Legion Upvote 0 Downvote
The only thing I can find on a quick Google search is some type of powder coating. Chris SolidWorks/PDMWorks 08 3.1 AutoCAD 08 ctopher's home (updated Aug 5, 2008) ctopher's blog SolidWorks Legion
Sep 29, 2008 Thread starter #3 chipgt500 Mechanical Joined Sep 25, 2008 Messages 3 Location US I was able to figure it out. It is Black Chrome plating, apparently used often in Japan. Now I just need to find a spec... Upvote 0 Downvote
I was able to figure it out. It is Black Chrome plating, apparently used often in Japan. Now I just need to find a spec...
Sep 29, 2008 #4 ctopher Mechanical Joined Jan 9, 2003 Messages 17,519 Location USA, CA Good luck. I have tried searching for their specs and usually hit a wall. If you work with a China mfg plant, they may have a copy. Chris SolidWorks/PDMWorks 08 3.1 AutoCAD 08 ctopher's home (updated Aug 5, 2008) ctopher's blog SolidWorks Legion Upvote 0 Downvote
Good luck. I have tried searching for their specs and usually hit a wall. If you work with a China mfg plant, they may have a copy. Chris SolidWorks/PDMWorks 08 3.1 AutoCAD 08 ctopher's home (updated Aug 5, 2008) ctopher's blog SolidWorks Legion
Oct 1, 2008 #5 Clyde38 Electrical Joined Oct 31, 2003 Messages 533 Location US Black Chrome Plating Specifications Mil-DTL-14538 http://www.reliableplating.com/blackchrome.html Upvote 0 Downvote
Oct 1, 2008 Thread starter #6 chipgt500 Mechanical Joined Sep 25, 2008 Messages 3 Location US Thanks Clyde38, that was the one I found as well. Upvote 0 Downvote