I have a drawing (in Japanese) that calls for a surface finish of "SBCr". The material is Nobinite CD-5 (similar to Invar 36). Does anyone know what process "SBCr" is referring to?
 
I was able to figure it out. It is Black Chrome plating, apparently used often in Japan. Now I just need to find a spec...
 
Thanks Clyde38, that was the one I found as well.
 