We need to buy carbon steel pipes with the following requirements:

Carbon should be equal or less than 0.20%, Carbon Equivalent should be equal or less than 0.40%, and (Cr+Ni+Cu) should be equal or less than 2%.

thanks

Luis marques
 
TomEun

Thank you for correcting me, it was my mistake (cr+ni+cu) might be less than 0.2%, not 2%.

A star for you!

It seems to me that you are familiar with these requirements, can you give-me a web site of a direct supplier, familiarized with these requirements?

It will be helpful

Regards