Our current supplier of a plastic molded thermoplastic polycarbonate urethane part is asking if we'd consider "upgrading" from a Arburg model 270S400-100 U press to a Arburg 270C-400-90. Differences provided by our supplier are listed below. We do not want to completely re-validate the process nor introduce changes that would impact our part performance (e.g., increase risk of degradation, etc.). I'm OK with the increased pressure and tonnage capacity. Also OK with "improved" controller. However, wasn't sure about intensification ratio. Based on quick research it sounds like the injection and hold pressures can be changed to account for change in ratio. Sound right? Should I ask more questions? Comments/advise appreciated.
Press Tonnage increasing from 40 to 44 tons
Maximum injection pressure hyd/electric increasing from 2000 to 2262 psi
Maximum hold pressure hydraulic increasing from 2000 to 2262 psi
Controller changing from Dialogica to Selogica
Intensification ratio changing from 18.1:1 to 16:1
Press Tonnage increasing from 40 to 44 tons
Maximum injection pressure hyd/electric increasing from 2000 to 2262 psi
Maximum hold pressure hydraulic increasing from 2000 to 2262 psi
Controller changing from Dialogica to Selogica
Intensification ratio changing from 18.1:1 to 16:1