I am a newbie in materials selection for petroleum production related project. I am having problems in selecting materials when the environment is highly conducive to pitting. Should I go for Duplex/Super Duplex/Alloy 625 or Alloy 825.

We will encounter very high CO2 and Cl-. Also, the operating temperature is around 90 C.
 
Replies continue below

Recommended for you

Hello Jbeckhou,

I appreciate your help. However, I am looking for "Performance" of the following steels in a specific environment (10 % CO2 (mol. fraction, 8000 mg/l Cl- ions and roughly 13000 MPa pressure):
1. Duplex Steels, 2. Super Duplex, 3. Alloy 625 and 4. Alloy 825.
I need to know the performance of the above steels when pitting and crevice corrosion are potential issues.

Best regards,
Samay
 
So you are looking for the Pren rating for the above materials?