Hi all,
A Sundyne LMV-311 (9500RPM) pump was recently removed for a leak on its degassing line. The pump itself did not fail however we used this opportunity to inspect the pump. During disassembly, the high speed shaft was inspected and wear and breakage on the splines were noticed. See picture attachment.
We are in the process of trying to determine the root cause of the shaft damage. Wear can be seen on all the splines and 1 spline is broken.
The pump has been operating at a constant (100% BEP) flow since its installation. Suction pressures and other parameters have been monitored and have been maintained within limits for the entire operation of the pump.
Please can anyone help with determining the cause/s of the damage?
Thank you.
A Sundyne LMV-311 (9500RPM) pump was recently removed for a leak on its degassing line. The pump itself did not fail however we used this opportunity to inspect the pump. During disassembly, the high speed shaft was inspected and wear and breakage on the splines were noticed. See picture attachment.
We are in the process of trying to determine the root cause of the shaft damage. Wear can be seen on all the splines and 1 spline is broken.
The pump has been operating at a constant (100% BEP) flow since its installation. Suction pressures and other parameters have been monitored and have been maintained within limits for the entire operation of the pump.
Please can anyone help with determining the cause/s of the damage?
Thank you.