Hello there, I'm trying to help with a side project following up a training HAZOP analysis where it's has been underlined how a PSV might be necessary for a loading pipeline where fluid might get trapped and be effected by solar heat. The fluid is diluite sulphuric acid (at different concentration depending on the request).
By looking at the Total Pressure of Aqueous Sulfuric Acid Solutions I've gathered that no vaporization of the solution has to be expected as the pressure would have to be too low.
By reading some very interesting threads here I understood how in this case a TRV should be required, so I've tried to evaluate what thermic expansion is to be expected to then understand what overpressure could be developed.
At this point I've calculated the cubic expansion coefficient α=0,0006 1/°C (both by hand and also by finding tabulated values) and also the isothermal compressibility coefficient X=3*10^-5 1/bar. By putting this informations together i get ΔP/ΔT=19 bar/°C so with only 1°C the pressure would increase of 19 bar, way higher than the 5 bar design pressure of the pipes.
Could this be correct ? Should i stick with the TRV or should I get a look into a proper PSV ? Many thanks in advance
By looking at the Total Pressure of Aqueous Sulfuric Acid Solutions I've gathered that no vaporization of the solution has to be expected as the pressure would have to be too low.
By reading some very interesting threads here I understood how in this case a TRV should be required, so I've tried to evaluate what thermic expansion is to be expected to then understand what overpressure could be developed.
At this point I've calculated the cubic expansion coefficient α=0,0006 1/°C (both by hand and also by finding tabulated values) and also the isothermal compressibility coefficient X=3*10^-5 1/bar. By putting this informations together i get ΔP/ΔT=19 bar/°C so with only 1°C the pressure would increase of 19 bar, way higher than the 5 bar design pressure of the pipes.
Could this be correct ? Should i stick with the TRV or should I get a look into a proper PSV ? Many thanks in advance