Sulfuric Acid Tanks 70-100%

Status
Not open for further replies.

Freddy1234

Civil/Environmental
Joined
Nov 7, 2012
Messages
1
Location
CA
Looking to install new sulfuric acid tank to replace the existing Ferrichem 30 tank we now have in services. The ferrichem requires s.s. or FRP. We would kike to install a FRP tank for the Sulfuric just encase we every have to go back to Ferrichem in the future. Is FRP ok for Sulfuric Acid 70%-90%
 
70% sulphuric aci is an upper threshold for FRP, so this isn't the way to go.
 
You can find many info consulting NACE Standard SP0294-2006 and NACE Standard RP0294-94
 